Skip to content

Microscopy technique sheds light on hydrogen’s effects in metal

Hydrogen, the second-tiniest of all atoms, can penetrate right into the crystal structure of a solid metal. That’s good news for efforts to store hydrogen fuel safely within the metal itself, but it is bad news for structures such as the pressure vessels in nuclear plants, where hydrogen uptake eventually makes the vessel’s metal walls more brittle, which can lead to failure. But this embrittlement process is difficult to observe because hydrogen atoms diffuse very quickly, even inside the solid metal.

Now, researchers at MIT have figured out a way around that problem, creating a new technique that allows the observation of a metal surface during hydrogen penetration. Their findings are described in a recent paper in the International Journal of Hydrogen Energy, by MIT postdoc Jinwoo Kim and Thomas B. King Assistant Professor of Metallurgy C. Cem Tasan.

The new way of observing the embrittlement process as it happens may help to reveal how the embrittlement gets triggered, and it may suggest ways of slowing the process—or of avoiding it by designing alloys that are less vulnerable to embrittlement.

The key to the new monitoring process was devising a way of exposing metal surfaces to a hydrogen environment while inside the vacuum chamber of a scanning electron microscope (SEM). Because the SEM requires a vacuum for its operation, hydrogen gas cannot be charged into the metal inside the instrument, and if precharged, the gas diffuses out quickly. Instead, the researchers used a liquid electrolyte that could be contained in a well-sealed chamber, where it is exposed to the underside of a thin sheet of metal. The top of the metal is exposed to the SEM electron beam, which can then probe the structure of the metal and observe the effects of the hydrogen atoms migrating into it.

The hydrogen from the electrolyte “diffuses all the way through to the top” of the metal, where its effects can be seen, Tasan says. The basic design of this contained system could also be used in other kinds of vacuum-based instruments to detect other properties. “It’s a unique setup. As far as we know, the only one in the world that can realize something like this, he says.

In their initial tests of three different metals—two different kinds of stainless steel and a titanium alloy—the researchers have already made some new findings. For example, they observed the formation and growth process of a nanoscale hydride phase in the most commonly used titanium alloy, at room temperature and in real time.

Devising a leakproof system was crucial to making the process work. The electrolyte needed to charge the metal with hydrogen, “is a bit dangerous for the microscope,” Tasan says. “If the sample fails and the electrolyte is released into the microscope chamber,” it could penetrate far into every nook and cranny of the device and be difficult to clean out. When the time came to carry out their first experiment in the specialized and expensive equipment, he says, “We were excited, but also really nervous. It was unlikely that failure was going to take place, but there’s always that fear.”

Tsuzaki adds that “once it is accomplished, outputs by this method would be super. It has very high spatial resolution due to SEM; it gives in-situ observations under a well-controlled hydrogen atmosphere.” As a result, he says, he believes that Tasan and Kim “will obtain new findings of hydrogen-assisted dislocation motion by this new method, solve the mechanism of hydrogen-induced mechanical degradation, and develop new hydrogen-resistant materials.”

The work was supported by the Exelon Corp through the MIT Energy Initiative’s Low-Carbon Energy Center for Advanced Nuclear Energy Systems.

************

Image – This illustration depicts the main elements of the system the team used: The multicolored slab at center is the metal layer being studied, the pale blue region at left is the electrolyte solution used as a source of hydrogen, the small blue dots are the hydrogen atoms, and the green laser beams at right are probing the process. The large cylinder at right is a probe used to indent the metal to test its mechanical properties. Courtesy of the researchers.

For more information:

mit.edu

Facebook
Twitter
LinkedIn