Nitrex, Nevada, has received certification from Honeywell for copper plating services. The copper plating supplied will mask selected areas of the metal part to prevent nitriding of the substrate surface. Honeywell is a global leader of aerospace parts and services supplying the commercial, defense, and space aircraft industries.
The Type II Copper plating is done following AMS 2418 as well as the customer’s specific specifications. The copper plating line at the Nevada facility can plate up to three rack loads and strip two rack loads of parts at the same time. Today the line processes parts for aerospace primes as well as Formula 1 Racing.
“The approval involved a stringent audit process that the experts at Nitrex went through diligently, which is something we always do, as part of our values and culture. In addition to copper plating, Nitrex HTS Nevada has also been approved by Honeywell for nitriding of stainless steels, steel alloys, and tool steels,” commented Joe Beal, Facility Manager of Nitrex Nevada.
“This additional approval from Honeywell reflects the growing recognition and value that Nitrex brings to the aerospace market – first with Nitreg nitriding services and today with copper plating. Our strength is our ability to work closely with customers, expand and adapt our capabilities to support them in their growth, and ultimately to ensure that their mission-critical applications are expertly serviced to meet or exceed in-service component performance. I want to thank our customers for their trust and business and congratulate the entire Nevada team for this accomplishment,” said Jason Orosz, president of Nitrex Heat Treating Services (HTS).