Solar Atmospheres vacuum heat treats longest nickel alloy tubes ever
Solar Atmospheres of Western Pennsylvania, Hermitage, Pa., successfully vacuum heat treated the largest and longest load of nickel alloy tubing ever in a commercial vacuum furnace. They were able to preserve the brightness and cleanliness of a 45-foot-long seamless tubing while meeting extremely stringent mechanical properties.