As part of a prestigious 2023 summer internship with the U.S. Department of Defense, John Migliore, a fourth-year Ph.D. candidate at The University of North Carolina at Chapel Hill departments of applied physical sciences and chemistry, conducted tests on whether high-performance polymers would change the mechanical and structural properties of ceramic materials.