Corrosion control by self-healing epoxy coatings

Scientists at the Instituto de Ciencia y Tecnologia de Polimeros (ICTP) and Centro Nacional de Investigaciones Metalurgicas (CENIM), Spain, studied corrosion control by autonomous self-healing epoxy coatings based on superabsorbent healing agents.