Why light poles failed in Hurricane Ian despite meeting design standards

A new University of Florida study reveals how hidden flaws in design and installation of aluminum light poles on a Central Florida bridge contributed to their unexpected collapse when Hurricane Ian moved across Florida in 2022, even though wind speeds remained below the structures’ design limits.