University of Michigan engineers have found that the light in OLED displays comes from nanoscale hotspots—some of which flicker—rather than from a perfectly uniform surface, a behavior that could shorten device lifespans by causing certain areas to carry more current and burn out faster. The studysuggests that these uneven emission patterns may also affect the performance of organic electronics such as solar cells and transistors. As a potential fix, researchers propose using crystalline instead of amorphous structures to improve durability. The work was supported by the U.S. Department of Energy and Universal Display Corp.
Charge rivers in hilly OLED energy landscapes
“The calculations that motivated us to look for this are actually pretty old. In the mid-2000s, people were predicting what they called a current channeling phenomenon,” said Chris Giebink, U-M professor of electrical and computer engineering and also senior author of the study. “You could liken it to a hilly landscape. The electrons, or charge carriers, that move through the device tend to want to follow the lowest energy pathways, so they’ll travel along the valleys.”
Charge carriers come in two flavors, electrons and positively charged “holes,” which run in opposite directions through the landscape. Where those rivers cross, light-emitting molecules convert electron-hole pairs into photons, or particles of light.
Because some valleys are deeper than others, they tend to support high-traffic rivers of charge carriers, with densities that are thought to be 10 to 100 times higher than the rest of the material. In contrast, crystalline materials are more uniform. Their landscape is flatter, leading the charge carriers to spread out more evenly, reducing the hotspot effect.
Spotting nanoscale hotspots with superresolution
Theory suggests that the hotspots are just a few tens of nanometers across. They appear as graininess in images from an optical microscope, which is limited to details of a couple hundred nanometers or bigger.
“An initial concern was whether we were seeing a microscope artifact,” said Joshua Springsteen, a Ph.D. student in electrical and computer engineering and first author of the study. “We examined the same area of the device with our microscope using both photoluminescence and electroluminescence, confirming that it was an electrical phenomenon.”
Because some of the lights flicker and aren’t always in sync, Springsteen could take a video of the device and run it through software that keyed in on the changes in brightness when one hotspot switched off while another stayed on. This technique, called superresolution optical fluctuation imaging, helped the team confirm that the hotspots were smaller than half the wavelength of the green light they emitted.
The researchers believe the blinking is due to charge carriers that are temporarily trapped in dips in the energy landscape. When that happens, they act more like dams, repelling other charge carriers, which seek alternate routes and cause downstream hotspots to go dark. Eventually, the charge carrier absorbs enough heat to pop back out of the dip, and the original hotspot lights up again. Because the flickering hotspots aren’t in sync, the human eye perceives amorphous OLEDs as glowing steadily.
To confirm that they had the mechanism right, the team used those earlier calculations that showed where charge-carrier rivers flow and meet. Springsteen took these theoretical freeze-frames and processed them to mimic the way the hotspots would have been blurred by the superresolution microscopy technique they used. These modified modeling images resembled the experimental images well enough that the team is confident they were seeing the hotspots.
The device was built in the Lurie Nanofabrication Facility and studied at the Michigan Center for Materials Characterization, both of which are operated and maintained with support from indirect cost allocations in federal grants.
For more information: Michigan Center for Materials Characterization
Image: Hotspots appear in an optical microscope image examining the surface of a green OLED, processed to quantify brightness. These hotspots may limit the lifetimes of amorphous OLEDs. Image: Joshua Springsteen, Optoelectronic Components and Materials Group, University of Michigan.