Hot Isostatic Pressing (HIP)

MPIF explains how heat and high gas pressure close internal porosity in metal parts, and why aerospace relies on it.

Thermo Fisher introduces new RaptIR X FTIR Microscope

Thermo Fisher Scientific (Waltham, Mass.) recently launched the Thermo Scientific Nicolet RaptIR X FTIR Microscope. The new equipment is the latest advancement in FTIR microscopy designed to make chemical analysis of microscopic samples more accessible, intuitive and efficient for laboratories.

Novel x-ray imaging tool for studying nuclear materials

A first-of-its-kind instrument at Brookhaven National Laboratory (Upton, N.Y.) combines four imaging techniques into one experimental setup, enabling comprehensive studies of materials for next-generation nuclear reactors.