The April issue of Advanced Materials & Processes magazine has an editorial focus on Materials Testing and Characterization.
IMS board member participates in key study to improve properties of steel
Movable silicon ‘lenses’ enable neutrons to see new range of details inside objects
The National Institute of Standards and Technology (NIST), the National Institutes of Health (NIH), and Canada’s University of Waterloo have developed an innovative way to focus beams of neutrons allowing scientists to probe the innards of opaque objects at a size range they were blind to previously. The new method allows for the interior examination of objects from meteorites to cutting-edge manufactured materials without damaging them.