Beryllium Chemistry and Processing

Author: Kenneth A. Walsh   |   Editor: David L. Olson ,Edgar E. Vidal, Edward Dalder, Alfred Goldberg, and Brajendra Mishra   |   Hardcover   |   Product code: 05223G   |   ISBN: 978-0-87170-721-5

Classified as: Environmental Impacts Metals and Alloys

Price: $257.00 Member Price: $191.00

A comprehensive reference guide to beryllium, its history, and its chemical, mechanical, and physical properties.

The 29 chapters include the mineralogy of beryllium and the preferred global sources of ore bodies. The identification and specifics of the industrial metallurgical processes used to form oxide from the ore and then metal from the oxide are thoroughly described. The special features of beryllium chemistry are introduced, including analytical chemical practices. Beryllium compounds of industrial interest are identified and discussed. Alloying, casting, powder processing, forming, metal removal, joining and other manufacturing processes are covered.

The effect of composition and process on the mechanical and physical properties of beryllium alloys assists the reader in material selection. The physical metallurgy chapter brings conformity between chemical and physical metallurgical processing of beryllium, metal, alloys, and compounds. The environmental degradation of beryllium and its alloys both in aqueous and high temperature condition are presented. The health and environmental issues are thoroughly presented the current requirements and established practices for handling beryllium in the workplace are available. A thorough list of references will assist the user of this book.