Element Hitchin, UK, successfully completed a groundbreaking proof-of-concept research project to design and build equipment for the continuous quality control and repairing of reinforced thermoplastic pipes during the manufacturing process.
Element Hitchin, UK, successfully completed a groundbreaking proof-of-concept research project to design and build equipment for the continuous quality control and repairing of reinforced thermoplastic pipes during the manufacturing process.