Lockheed Martin, Sunnyvale, Calif., announces that the U.S. Navy’s first 3-D-printed missile component, a part called a connector backshell, made its debut on three Trident II D5 Fleet ballistic missiles.
IBC Advanced Alloys Corp., Vancouver, has signed an agreement with a leading global manufacturer of semiconductor and electronics assembly equipment to be its exclusive supplier of Beralcast beryllium-aluminum cast components.
Phoenix Temperature Measurement, Clearwater, Fla., announces that a major steel coil manufacturer has taken delivery of a ‘hot box’ system to monitor the temperature of steel wire coils through their annealing process.
Paulo Products Co., St. Louis, Mo., announces that its Kansas City Division is now AS9100 certified, and joins the Cleveland Division in being both AS9100 certified and Nadcap accredited.