Norsk Titanium, Norway, recently announced agreements with Mecachrome, Thales, Boeing, and the state of New York regarding its Rapid Plasma Deposition (RPD) additive manufacturing process. Norsk says that these titanium parts have strengths equivalent to those of forgings, but at lower cost and shorter design-to-market times.