A simple fabrication technique derived by engineers at Massachusetts Institute of Technology, Cambridge, may help chocolate artisans create uniformly smooth shells and precisely tailor their thickness.
A 3D printer allows researchers at Ames Laboratory, Iowa, to rapidly create and assess alloys of varying composition to find just the right combination to produce materials with the desired characteristics.
AMG Advanced Metallurgical Group N.V, Amsterdam, announces that AMG Titanium Alloys and Coatings (AMG TAC) has been selected by MTU Aero Engines to provide titanium aluminides for the production of the Pratt & Whitney PurePower PW1100G-JM engine.
The Royal Institute of Technology in Stockholm announces that its researchers have developed a quality assurance method for welds in high-strength steel in which a laser profile scanner assesses the welded surface and measures the quality of the weld.
Solar Manufacturing, Souderton, Pa., announces that it has been cooperating for the past year with Graphite Machining Inc., Topton, Pa., on the development and testing of a new graphite board material and its application in vacuum furnace hot zones.