Although handheld spraying has been carried out for nearly a century, it is not the preferred or safest means of spraying; motion control is necessary to ensure operator safety and coating quality.
Fleet Readiness Center East, a US Navy aviation repair and maintenance facility, Havelock, North Carolina on Marine Corps Air Station Cherry Point, marked a milestone with the induction of the first F-35B Lightning II aircraft to undergo laser peening modifications.
Scientists at Fraunhofer IWS Dresden, Germany, have developed a cost-effective HICLAD process to maximize corrosion and wear protection that also reduces particulate emissions, important as brake discs are moving into focus as part of current green-energy discussions.
Mitsubishi Heavy Industries, Ltd. (MHI), Tokyo, has determined the recipients of its 2020 “Best Innovation” awards, an in-house program to recognize activities that contribute to the conservation and protection of the global environment, and the lowering of environmental loads.
3D Systems, Rock Hill, South Carolina, has been selected by Raytheon Technologies and the Army Research Laboratory to optimize a component relative to an Army modernization product to maximize cooling and improve overall system performance.