Researchers at the U.S. Department of Energy’s Argonne National Laboratory, Lemont, Ill., developed a new technique that accelerates the solving of material structures from patterns uncovered in x-ray experiments.
Leading semiconductor test equipment supplier Advantest Corp., Japan, announced the latest addition to its extended power supply card series: the DC Scale XPS128+HV, developed to lower the cost of testing for power management ICs and other high-voltage devices.
American Elements announced that its engineers have invented a novel nanoscale electrolyte material for use in cutting-edge lithium-sulfur battery technology.
A new study by the University of Amsterdam’s Institute of Physics and research institute AMOLF tested how well artificial intelligence (AI) can estimate the properties of so-called combinatorial mechanical metamaterials.