Graphene goes into silicon at room temperature

Materials researchers at North Carolina State University, Raleigh, developed a technique that allows the integration of graphene, graphene oxide (GO), and reduced graphene oxide (rGO) onto silicon substrates at room temperature by using nanosecond pulsed laser annealing.