A team of chemists has developed a method to yield highly detailed, 3D images of the insides of batteries. The technique, based on magnetic resonance imaging (MRI), offers an enhanced approach to monitor the condition of these power sources in real time.
ASM Appoints New Managing Director
Bodycote acquires Nitrex Metal Technologies for precision gas nitriding
Chromium Nitride in Duplex Stainless Steels
Because of the use of nitrogen as an alloying element in these stainless steels, chromium nitrides (CrN) may be present on α/α grain boundaries, on γ/α boundaries, and within the α grains. If formed in large quantities and under conditions in which the chromium-depleted areas do not have time to repair themselves during annealing, the presence of CrN may adversely affect corrosion resistance.