Spray Tips: Fluidized-bed systems

Other commonly used gravity-based powder-feeding systems for feedstock delivery are fluidized-bed systems, where the powder feedstock is suspended by an upward flow of gas, creating a fluid-like state that allows for consistent and controlled delivery of the powder to the process.