Spray Tips: Basic Design of a dc Plasma Arc Gun

The basic components and design of a dc plasma arc gun are illustrated in the diagram. Direct-current plasma arc guns combine an axially aligned cathode, an anode/nozzle, and some means to control gas flow geometry in the arc chamber.

Buehler upgrades Wilson DiaMet hardness testing software

Buehler, Lake Bluff, Ill., announces that it has extensively upgraded its Wilson DiaMet hardness testing software with features designed to facilitate and accelerate specific applications, such as the documentation of the hardness distribution in welds, or the depth of hardening in induction-hardened workpieces or in objects hardened by conventional processes.