Wisconsin Oven Corp., East Troy, Wis., announces the shipment of four electrically heated, enhanced duty, walk-in ovens to an automotive parts manufacturer for age-hardening aluminum parts.
Lindberg/MPH, Riverside, Mich. has completed shipment of a gas fired aluminum stack melting and holding furnace, providing a manufacturer of recreational vehicles the additional melt capacity for a new diecasting machine.
Integer Holdings Corp., Frisco, Texas, has completed the previously announced sale of its Advanced Surgical and Orthopedics (AS&O) product lines to MedPlast LLC for $600 million in cash.
Fort Wayne Metals, Fort Wayne, Ind., announces that its engineers have developed a non-inclusion-based process for shape memory alloy fatigue durability enhancement.