NASA, Boeing engineers investigate shape-memory alloys to bend aircraft wings in flight

NASA, Washington, announces that a team of engineers working within its Spanwise Adaptive Wing (SAW) project is investigating the feasibility of bending or shaping portions of an aircraft’s wings in-flight, potentially increasing performance and efficiency by reducing weight and drag. The innovative actuation system that NASA and engineers from the Boeing Company are developing is […]