NIST releases guide to fractography of ceramics and glasses

NIST, Gaithersburg, Md., has released a new, expanded edition of the NIST Recommended Practice Guide, “Fractography of Ceramics and Glasses” (NIST Special Publication 960-16e2), a guide developed to help engineers and scientists analyze the patterns in fractures of ceramics and glasses.

Electron Beam Additive Manufacturing

Sciaky’s Electron Beam Additive Manufacturing (Ebam) is a 3D printing technology that excels at producing large-scale, high-value metal parts.