The University of Southern California, Los Angeles, announces that a novel 3D-printing process called selective separation sintering has won the NASA competition for a technology that could enable space travelers to build structures of crushed basalt rock and regolith found on Mars.
3D printing gives Navy an edge
The best part about 3D printing, according to our sailors, is that there are few limitations. The freedom to design and print what you need, when you need it (without waiting for the supply chain) can increase our warfighters’ mission readiness and combat capability. Hear from sailors, engineers, and scientists about why additive manufacturing is so important for the Navy’s mission.