An international research group led by scientists at NIST’s Center for Nanoscale Science and Technology developed a method for measuring crystal vibrations in graphene
A quantum mechanical transport phenomenon demonstrated for the first time in synthetic, atomically-thin layered material at room temperature could lead to novel nanoelectronic circuits and devices, according to researchers at Pennsylvania State University, College Park.
A new polyimide aerogel developed at NASA’s Glenn Research Center, Cleveland, represents a revolutionary advance over the fragile silica aerogels currently on the market.
Forty years after the Air Force’s B-1 bomber took flight with a fixed cycle engine that would later power the first Boeing 737s and Airbus A320s, new propulsion technologies developed for the 737MAX and A320neo will form the core of next-gen combat aircraft.
Forty years after the Air Force’s B-1 bomber took flight with a fixed cycle engine that would later power the first Boeing 737s and Airbus A320s, new propulsion technologies developed for the 737MAX and A320neo will form the core of next-gen combat aircraft.