Researchers from North Carolina State University, Raleigh, report that they have fabricated stretchable transparent conductors that work because of their “nano-accordion” design.
The Technical University of Munich (TUM) announces that its researchers have printed razor-thin polymer electrodes with improved electrical properties.
Luminescent signals from green glowing diamond defects could monitor temperature in a range of physical and biological systems with unprecedented versatility