A research team at the University of Virginia School of Engineering and Applied Science, led by Assistant Professor Liheng Cai and his Ph.D. student Jinchang Zhu, has developed biomaterials with controlled mechanical properties that match various human tissues, potentially serving as the first building blocks for human-compatible organs printed on demand. Zhu highlighted this advancement […]
Chatbot Terms of Use
ASM Chatbot Terms of Use This Agreement is a contract between an ASM Chatbot user (“User” or “Users”) and ASM International, Inc. (“ASM”) (each a “Party”, and collectively the “Parties”). This Terms of Use (“Agreement”) governs the use of ASM International Inc.’s “ASM Materials Information Chatbot” (hereinafter “ASM Chatbot”) feature and is effective upon the […]
Wisconsin Oven ships electrically heated drop bottom furnace to the aerospace industry
Wisconsin Oven, East Troy, WI, announces that it has shipped an Electrically Heated Drop Bottom Furnace with a traveling quench tank and maintenance platform to the aerospace industry. This system will be used for the solution heat treatment of aluminum parts. The drop bottom furnace has a maximum operating temperature of 1,100°F and effective workspace […]
One Minute Mentor: Distortion in Tool Steels
Some of the main interactions that occur during the heat treatment of steel alloys including temperature, microstructure, and stress/strain. Especially for tool steels these interactions are mainly influenced by the carbon content in the steel matrix, the types and relative amounts of the alloying elements, and the carbide formation/transformation/precipitation characteristics of the alloy system. Heat […]
Harper International Receives Order for Scientific Line for Pitch Carbon Fiber
Harper International, Buffalo, NY, announces that it has been awarded a contract to engineer and manufacture a Scientific Line for the production of Bitumen Pitch Carbon, which will be installed at Alberta Innovates, located in Edmonton, Alberta, Canada. The facility will be operated by InnoTech Alberta, a wholly-owned subsidiary of Alberta Innovates. The equipment delivery […]