Students build low-cost cold spray metal 3D printer prototype

Rice University students in Houston, Texas, have developed a cold spray metal 3D printing device that uses pressure and velocity instead of temperature, potentially expanding the capabilities and reducing the costs of metal additive manufacturing and repairing for complex, one-off parts.