Nitrex Metal, Canada, has sold a second NX-815 E furnace to Elvial, one of the largest aluminum extrusion companies in Greece. This will help ELVIAL meet the needs created by their plant expansion and to increase their manufacturing capacity.
Recreating deep-earth conditions to see how iron copes with extreme stress and pressure
Measuring what happens during the collision of celestial bodies or at the Earth’s core is obviously not very practical. But researchers at the Department of Energy’s SLAC National Accelerator Laboratory have now observed for the first time how iron’s atomic structure deforms to accommodate the stress from the pressures and temperatures that occur just outside of the inner core.