There are three basic types of grit-blasting equipment: pressure machines or pressure pots, suction-type nozzles, and centrifugal or airless blasting machines.
Wall Colmonoy, Madison Heights, Mich., is providing solutions to increase the lifetime of key operational equipment for UK steel manufacturers by laser cladding reheat furnace skid posts with Colmonoy 625.
Precision Coating, Hudson, Mass., a leading medical coatings service provider to interventional, orthopedic, and advanced surgical markets, announced a merger with N2 Biomedical, a Bedford, Mass.-based company.
Impact Innovations GmbH, Germany, collaborating with Airborne Engineering, a UK based company specializing in propulsion system design and testing, demonstrated its cold spray additive manufacturing process is suitable for combustion chambers for commercial rocket engines.