Flame-sprayed silver protects 40-ton generator rotor

RFI Screening Ltd., England, has selected Metallisation MK61 Flamespray equipment from Metallisation Ltd., England, to metal spray a 40-metric-ton generator rotor with fine silver.  It was first sprayed with a 25-micron coating of molybdenum, to optimize the adhesion of the top coat of silver.  A final coating of silver was then added to achieve the specified outside diameter on the shaft. In a typical application, a coating 250 microns thick of silver would be sprayed.

Sensing element made via MIM for auto engines wins Grand Prize at PowderMet 2013

Indo-US MIM Tec Pvt. Ltd., Bangalore, India, earned a grand prize at PowderMet 2013 in the automotive engine category for a sensing element, a threaded port, and a support ring made for Sensata Technologies Holland B.V., Almelo, the Netherlands. Fabricated via MIM of 17‐4 PH stainless steel, the parts have a heat‐treated yield strength of 160,000 psi and ultimate tensile strength of 178,000 psi.

MPIF sponsors Additive Manufacturing conference

The Metal Powder Industries Federation (MPIF), Princeton, N.J., announces the inaugural conference on Additive Manufacturing with Powder Metallurgy (AMPM), May 18-20, 2014, at the Walt Disney World Dolphin Hotel, Orlando, Florida.   This specialized conference will be co-located with the PM2014 World Congress on Powder Metallurgy & Particulate Materials and the Tungsten, Refractory & Hardmaterials Conference, which will all be taking place under one roof in Orlando.

Diamond powders encapsulated in metal increase life of diamond compacts

Powdermet  Inc., Euclid, Ohio, offers DiaBond, a family of engineered diamond powders specially designed to improve bonding in metallic matrices, including nickel-, cobalt-, copper-, and aluminum-based binders. DiaBond powders are comprised of diamond grains encapsulated in a 1-20 micron coating of cobalt, nickel, chromium, chromium carbide, tungsten, tungsten carbide, copper, aluminum, silicon, or rhenium.

Gold nanoparticles in polyurethane have high conductance and flexibility

Engineers at the University of Michigan, Ann Arbor,  report that networks of spherical gold nanoparticles embedded in polyurethane elastic materials may make the best stretchy conductors yet. The team discovered that the gold nanoparticles align into chain form, making excellent conductive pathways, when the polyurethane is stretched. Flexible electronics have a wide variety of possibilities, from bendable displays and batteries to medical implants that move with the body.