Jeol USA, Peabody, Mass., introduces the new JSM-7200F FE SEM with ultrahigh spatial resolution of 1.6 nm at 1.0 kV, and high probe current of 300 nA.
Global Foundries launches 22FDX semiconductor technology for ultralow-power devices
Physicists take a picture of magnetic waves
Pressure causes osmium to change state of matter
Using metallic osmium (Os) in experimentation, an international group of researchers demonstrated that ultra-high pressures cause core electrons to interplay, which results in experimentally observed anomalies in the compression behavior of the material. Os is one of Earth’s most exceptional elemental materials, possessing the highest known density at ambient pressure, one of the highest cohesive […]
Expo sells out for Heat Treat
The ASM Heat Treating Society announced that the exposition for Heat Treat 2015 has sold out for the second time in a row. Hundreds of heat treating companies and gear manufacturers will be displaying their latest and greatest products and services next month at the 28th annual ASM Heat Treating Society Conference and Exposition in […]