MATERIALS PARK, Ohio (October 1, 2024) – ASM International, the world’s largest association of materials-centric engineers and scientists, proudly announces that Dr. Navin Manjooran has been appointed President of the ASM International for the 2024-2025 term. With more than two decades of global leadership and technical expertise, Dr. Manjooran brings a wealth of knowledge in […]
One Minute Mentor: Distortion of High-Speed Steels
High-speed steels show a typical distortion behavior depending on the heat treatment parameters. The figure shows the change in length of cylindrical bars (diameter = 20 mm, or 0.8 in.) and length = 140 mm, or5.5 in.), with rolling direction longitudinal to the sample) for various heat treatment conditions with austenitizing, salt bath quenching, and […]
Bodycote presented aerospace materials solutions at Farnborough International Airshow
Bodycote, Macclesfield, U.K., participated in the 2024 Farnborough International Airshow, held this summer. Bodycote showcased its advanced thermal processing solutions specifically designed for the aerospace industry. The airshow, a key event for aerospace innovation, emphasizes themes like sustainability, future flight, and workforce development, providing Bodycote with a platform to highlight its role in enhancing the […]
Constellium celebrates the grand opening of its new recycling center in France
Constellium, Paris, announced the grand opening of its new advanced recycling center in Neuf-Brisach, France. The €130 million investment, supported by a grant from the France Relance investment program, is aimed at boosting Constellium’s presence in the automotive and packaging industries while fostering a circular, sustainable economy. The new facility will increase the plant’s recycling […]
SECO/WARWICK supplies vacuum furnaces to Huake Casting Control Technology Co., Ltd.
SECO/WARWICK, Meadville, PA, will provide a horizontal vacuum heat treatment furnace equipped with a graphite heating chamber and a 15 bar absolute gas quenching system. The furnace will be used by the Chinese manufacturer to produce components for the aviation and energy industries. The Vector furnace, known for its versatility and modular design, is a […]