Fluid-enhanced crystal engineering increases thin-film conductivity by a factor of ten

A team from the U.S. Department of Energy’s National Accelerator Laboratory and Stanford University, Calif., have developed a printing process they call FLUENCE-fluid-enhanced crystal engineering-that for some materials results in thin films capable of conducting electricity ten times more efficiently than those made by conventional methods. The printing method is fast and works with a variety of organic materials.

Strong thermal management composite made of graphite ligaments in titanium powder

Engineers at Oak Ridge National Laboratory, Oak Ridge, Tenn., have succeeded in consolidating ground graphite foam ligaments in titanium powder to make disks up to 7 inches in diameter with bulk thermal conductivity of 240 W/m-K, as well as high strength. The ground ligaments are about 500 microns thick and range in length from 100 to 200 microns.

Automated AFM system enables automatic defect and surface roughness review for semiconductors

Park Systems, Santa Clara, Calif., introduces Park NX-HDM, a fully automated atomic force microscopy (AFM) automatic defect review and sub-angstrom surface roughness measurement system for device substrates and disk media. The system increases throughput by up to 1000%, and offers a 30% higher success rate than prior systems. It analyzes, identifies, and scans media for all wafer sizes up to 150 mm.

Zinc oxide enhances antibacterial properties of dental resin

Researches lead by Sara Tavassoli at Shahed University, Tehran, Iran, wanted to create a composite resin with antibacterial properties without reducing its mechanical and physical properties.  “Zinc oxide nanoparticles were added to a preventive and treatment material and its antibacterial, mechanical, and physical properties were investigated at the same time,” she said.    Adding zinc oxide nanoparticles to the resins increased the antibacterial properties.

Sulzer Metco laser cladding system applies deposits on multi-dimensional surfaces

Sulzer Metco, Switzerland, introduces MetcoClad, a robotics-based laser cladding system that can apply welded deposits on multi-dimensional surfaces in a single cladding run. The robust systems simplify operability, reduce production set-up time, and monitor the cladding process. Part manipulation can be tailored to customer requirements.