Buehler, an ITW Company, Lake Bluff, Ill., introduces the PlanarMet 300, a new compact benchtop planar grinder built for fast and efficient grinding with high flatness and maximum edge retention.
Karlsruhe Institute of Technology (KIT), Germany, reports that its engineers are now working on low-pressure carbonitration, a process for the case hardening of low-alloy steel with methylamine.
Lindberg/MPH, Riverside, Mich., announces the shipment of an electric immersion aluminum holding furnace for a leader in the automotive parts industry to maintain aluminum at the required temperature for die casting.
Buehler, Lake Bluff, Ill., an ITW company, created the fully automatic Wilson VH3300 Vickers/Knoop hardness test system to meet virtually any requirement in the area of automated precision micro hardness testing.