Physicists detect elusive ‘Bragg glass’ phase with machine learning tool

Cornell quantum researchers have detected an elusive phase of matter, called the Bragg glass phase, using large volumes of x-ray data and a new machine learning data analysis tool. The discovery settles a long-standing question of whether this almost–but not quite–ordered state of Bragg glass can exist in real materials. The lead author is Krishnanand […]