Titomic achieves DNV qualification for oil & gas

Titomic Limited, Australia, has received a Statement of Qualification from Det Norske Veritas to use its low- and medium-pressure systems for applying protective, corrosion-resistant aluminum coatings in the field for the oil and gas sector.

Better metals are now possible through a novel analysis method

In a new study, researchers from Yale University (New Haven, Conn.) show that a mold about half the size of a fingernail could lead to the development of stronger, higher-performing materials for airplanes and other uses. Their novel method provides unique insight into the microstructure and properties of a metal and eliminates the limitations of more traditional analysis.