New material holds promise for low power electronics

Scientists have successfully paired ferroelectric and ferrimagnetic materials so that their alignment can be controlled with a small electric field at near room temperatures, an achievement that could open doors to ultralow-power microprocessors, storage devices, and next-generation electronics.

Constellium and UACJ joint venture to open aluminum sheet plant

Constellium N.V., Paris, and UACJ Corp., Japan, announce the official opening of their new manufacturing plant in Bowling Green, Kentucky, to supply aluminum automotive body sheet to the North American automotive industry under their joint venture, Constellium-UACJ ABS LLC.