The University of Warwick, England, announces that a team of researchers has discovered that the amount of oxide that forms at the surface of automotive high-strength steels depends on the ratio between manganese and additional alloying elements.
AK Steel, Westchester, Ohio, launches its Nexmet 440EX high-strength steel that provides greater ductility, strength, and formability for automotive applications.
Aleris Corp., Cleveland, Oho, a global aluminum rolled products producer, announces that it has entered into a definitive agreement to be acquired by Zhongwang USA LLC, a Chinese company.
The exposure of duplex stainless steels to temperatures in the range of 1100 to 1850°F can result in the formation of undesirable intermetallic compounds such as σ and χ phases.
For the Rio Olympics 2016, the 5130 Olympic and Paralympic medals were produced in Casa da Moeda do Brasil, the country’s mint — alongside its currency