Striking semiconductors with light in the furnace could reduce defects

The University of Utah, Salt Lake City, and the National Renewable Energy Laboratory, Golden, Colo., report that its researchers have discovered that if light is shone on semiconductor alloys as they are fired in a furnace at high temperatures, the light generates extra electrons that could suppress the growth of defects.