Instron, Norwood, Mass., celebrated its 70th anniversary on March 15, 2016, marking continued success in providing customers with the highest quality products, expert support, and world-class service.
Wisconsin Oven Corp., East Troy, Wis., has shipped two direct gas-fired batch ovens with load capacity of 6000 pounds each to a leading automotive supplier for tempering tire molds to produce longer mold life.
The Massachusetts Institute of Technology, Cambridge, reports its researchers have found that, at least in some nuclear reactors, adding less than 2% carbon nanotubes to aluminum can dramatically slow the breakdown process that causes it to become porous and brittle.