ASM International, Materials Park, Ohio, announces that organizers for Heat Treat Mexico are currently seeking abstract submissions on heat treating topics for the upcoming new event in Queretaro, Mexico, to be held later this year in September.
Liquidmetal Technologies Inc., Rancho Santa Margarita, Calif., has developed the Liquidmetal Hybrid Knife, manufactured of LM105 amorphous alloy by the Liquidmetal process.
NASA Goddard Space Flight Center, Greenbelt, Md., announces that one dozen beryllium mirrors have been installed on NASA’s James Webb Space Telescope, out of the eighteen mirror segments that make up the primary mirror.
Lawrence Berkeley National Laboratory, Berkeley, Calif., has reportedly developed an alloy composed of chromium, manganese, iron, cobalt, and nickel that becomes stronger and tougher at low temperatures.
Alcoa, Pittsburgh, has signed a long-term contract with GE Aviation for jet engine components made of advanced nickel-based superalloys, titanium, and aluminum for a broad range of GE Aviation engine programs.