Purdue University, West Lafayette, Ind., announces that a team of its engineering students, faculty, and staff has designed and built the torches for the 2016 Indiana Bicentennial relay.
Ipsen, Cherry Valley, Ill., reports that a Midwest commercial heat treater recently purchased an Atlas atmosphere furnace for several processes, including carburizing, neutral hardening, and carbonitriding, as well as to help the company further increase its capabilities and product offerings.
Argonne National Laboratory, Argonne, Ill., reports that its engineers have learned that the structure of graphite, its spatial arrangement in cast iron, and its phase connectivity are key factors that determine the properties of cast iron.
Imec, Belgium, and Coventor, Cary, N.C., announce the expansion of a joint development project to explore process variation issues in 7 nm semiconductor technology.