Researchers at the U.S. Department of Energy’s Argonne National Laboratory have overcome a critical barrier in diamond-based electronics and microelectronics by using nanotechnology to integrate two-dimensional materials for efficient n-type doping, a breakthrough in electronic materials designed to operate in high-temperature environments and other harsh environments.