The boards of directors of Berkshire Hathaway Inc., Omaha, Neb., and Precision Castparts Corp., Portland, Ore., have unanimously approved a definitive agreement for Berkshire Hathaway to acquire all outstanding PCC shares for $235 per share in cash.
Applied Materials Inc., Santa Clara, introduces the Applied Olympia ALD (atomic layer deposition) system featuring a unique, modular architecture that delivers high-performance ALD technology to manufacturers of leading-edge 3D memory and logic chips.
Materion Performance Alloys, Mayfield Heights, Ohio, has more than doubled its capacity to produce foil gauge ToughMet alloys that are used to make the company’s BrushForm 158 copper-nickel-tin alloy strip product line.
Researchers at the Center for Integrated Nanostructure Physics at Sungkyunkwan University, South Korea, report that they have developed a high-performance transistor made of black phosphorus (BP).