Austenitizing is the heat treatment in which the final alloy element partitioning between the austenitic matrix (which will transform to martensite) and the retained carbides occurs.
Linde highlights advanced technologies at Heat Treat 2015
Linde LLC, Murray Hill, N.J., will showcase advanced gas control technologies and engineering services for heat treatment furnaces at Heat Treat 2015 next week in Detroit, booth 248.