Engineers from Treibacher Industrie AG, Austria, presented a discussion titled “Engineered YSZ Powders for High Power Plasma Spraying of Thermal Barrier Coatings” at the ASM International ITSC 2019 conference.
High-speed laser cladding enables surface speeds up to 400 m/min with less heat
Scientists from Höganäs, Sweden, presented “High-speed laser cladding for innovative applications” at ASM International’s ITSC 2019 conference in Japan.