Prevention of Harassment and Discrimination Policy

Board Policy Number: 10.50 Code of Conduct and Anti-Harassment Policy Purposes ASM International (“ASM”) is committed to providing a professional environment that is free from harassment and discrimination in which all individuals, including members, employees, and volunteers, are treated with respect and dignity. Each individual has the right to be in a professional atmosphere free […]

One Minute Mentor: Dimensional Stability in Through-Hardening Bearing Steels

Dimensional stability is a bearing condition of great concern. This means heat treating is conducted to prevent excessive diametral growth in the bearing due to retained austenite transforming to martensite at elevated or subzero service temperatures, or shrinkage due to continued tempering of the martensite at high service temperatures.