Bodycote receives Cameron Schlumberger approval for coatings

Bodycote, UK, has announced that their coating solutions have been approved by Cameron Schlumberger. The approval recognizes Bodycote’s Knowsley facility as a center of excellence for providing thermal coatings and K-Tech ceramic coating solutions to oil & gas and industrial gas turbines.

High-throughput method of identifying novel materials

Coupling computer automation with an ink-jet printer originally used to print T-shirt designs, researchers at Caltech and Google have developed a high-throughput method of identifying novel materials with interesting properties.