Researchers from the Center for Thermal Spray Research, Stony Brook University, N.Y., reported on thermal spray techniques for restoring heavy machinery in Infrastructure and Heavy Machinery Restoration Enabled Via Spray Processing: Lifecycle Design, Structural Reclamation, and Methods For Evaluation, at the ITSC 2018 conference in May.
How “big data” can help with the design of thermal spray coatings for power generation
HVAF flash carbide enables thermal spray of thin hard coatings that could replace chromium
Researchers from Kermetico Inc., Benicia, Calif., and H.C. Starck, Germany, discussed the latest developments in HVAF Flash Carbide as Economical Alternative to Electroplated Hard Chrome at the ITSC 2018 conference in May.
Dr. Patrice Turchi Selected as the 2019 Recipient of the J. Willard Gibbs Phase Equilibria Award
ASM is pleased to announce that Dr. Patrice Turchi, Senior Scientist, Lawrence Livermore National Laboratory, Livermore, CA, is the 2019 J. Willard Gibbs Phase Equilibria Award recipient. His citation reads: “For outstanding and pioneering contributions in the application of first-principles, quantum-mechanical calculations to the modeling of phase equilibria and thermodynamic behavior of alloys.” The Gibbs Award […]
Electric Power Research Institute explains high-altitude electromagnetic pulses (HEMP)
High-altitude electromagnetic pulse (HEMP) refers to the electromagnetic pulse that is created by the high-altitude detonation of a nuclear weapon. Numerous stakeholders assert that a HEMP attack is probable, and its impact would be catastrophic to the power system infrastructure. However, a science-based approach is needed to assess the true impact of this threat.